Knit Fabric Manufacturer Since 2009 · China

Knit Fabric Dyeing and Finishing Process: From Greige to Finished Roll

Knit Fabric Dyeing and Finishing Process: From Greige to Finished Roll
Table of Contents
Add as a preferred source on Google

Find our technical articles, sourcing guides and industry insights more easily.

Knit fabric dyeing and finishing turns greige fabric from the circular knitting machine into a finished roll with an agreed colour, width, GSM and shrinkage. Most circular knits go through ten steps: inspection, pretreatment, dyeing, washing-off, dewatering, heat setting, compacting, four-point inspection, lab testing and packing. Each step fixes one property, so most bulk faults can be traced back to a single step.

What is knit fabric dyeing and finishing?

Dyeing and finishing, often called wet processing, is the set of chemical and mechanical treatments that makes greige knit fabric ready for cutting. It covers three jobs: pretreatment cleans the fabric so dye takes evenly, dyeing gives it one uniform colour, and finishing sets its width, weight, shrinkage and hand feel. Printing follows a separate route and is not covered here; see how reactive, pigment and sublimation prints differ.

Knits need gentler handling than wovens. Their interlocking loops stretch under tension, so circular knits are usually processed in tube or rope form on low-tension machines, and finishing has to bring the loops back to a relaxed, stable shape.

The ten steps at a glance

The same ten steps apply to most circular knits; fibre content changes what happens inside some of them.

StepWhat happensWhat it controls
1. Greige inspection and batchingKnitting faults are checked; rolls are grouped into dye lotsFaults caught before dyeing; lot consistency
2. PretreatmentScouring and bleaching, or pre-setting for syntheticsEven dye uptake, whiteness
3. DyeingDye is applied in jet or overflow machinesColour and shade match
4. Washing-offUnfixed dye is rinsed and soaped off; softener addedWash and rubbing fastness
5. Dewatering and slittingWater is removed; the tube is slit if finished open-widthEven drying, straight edges
6. Drying and heat settingFabric is dried and set to width on a stenterWidth, GSM, stability
7. Compacting or special finishesLengthwise compaction; brushing or mercerising if orderedLength shrinkage, hand feel
8. Four-point inspectionEvery roll is checked and gradedVisible defects
9. Lab testingSpecimens from the bulk lot are testedFastness, shrinkage, pilling
10. Rolling and packingRolls are measured, labelled and packedTraceability

Why fibre content changes the route

Fibre content decides which steps a fabric needs and how hot they can run. Across the 5,833 fabrics in our development library (ERP snapshot, 26 October 2026), the share that needs each kind of handling is:

Fibre contentShare of our libraryWhat it changes in the route
Polyester, nylon or spandex80%Needs heat setting to hold width and shape
Spandex53%Caps the setting temperature so the fabric keeps its stretch
A cellulosic fibre (cotton, viscose) with polyester or nylon42%Each fibre takes its own dye class, usually in two dyeing stages

This is why the full fibre content, not just the main fibre, should be confirmed before a dyeing route and price are agreed.

Step 1: Greige inspection and batching

Faults are cheapest to catch before dyeing, because dyeing makes holes, dropped stitches and needle lines more visible, not less. After inspection, rolls that will be dyed together are grouped into one dye lot and sewn end to end into a continuous rope for the dyeing machine. Fabric from one lot matches most closely, so an order that needs one consistent shade across many rolls should say so before production starts.

Step 2: Pretreatment

Pretreatment removes whatever would stop dye from taking evenly. Cotton is scoured to remove natural waxes and knitting oil, usually together with hydrogen peroxide bleaching close to the boil; whites and pastels need a full bleach, while dark shades may only need scouring. Polyester, nylon and spandex knits carry little natural impurity, so the main tasks are removing oil and, often, pre-setting the fabric on a stenter so it does not crease or shrink in the hot dye bath.

Step 3: Dyeing

Each fibre needs its own dye class. Most circular knit fabric is dyed in rope form in jet or overflow machines, using reactive dyes for cotton and other cellulosics, disperse dyes for polyester at about 130 °C, and acid dyes for nylon; blends take one dye class per fibre.

Before bulk dyeing, the colour is matched as a lab dip: a small dyed sample approved against the buyer's colour standard, which then becomes the reference for the bulk lot. Bulk shade can still move if liquor ratio, heating profile or pretreatment differ from the lab; see why bulk shade can drift after approval.

At Runtang

Lab dips are made on three Datacolor systems with automatic dye dispensing, usually within 3–5 working days, with options A, B and C for each colour. They are checked under the light sources the buyer names, such as D65, TL84 and CWF (our colour approval steps and timings). Bulk dyeing runs on 80 high- and low-temperature dyeing machines with 230 tubes, with capacity of up to 150 tons a day; the high-temperature machines handle polyester.

Automatic dye dispensing system in a colour matching laboratory
Our colour lab, where lab dips are matched with automatic dye dispensing before bulk dyeing.

Steps 4–5: Washing-off, dewatering and slitting

Washing-off largely decides wash and rubbing fastness. After dyeing, the fabric is rinsed and soaped to remove dye that has not bonded to the fibre, and dark polyester shades also get a reduction-clearing wash. The fabric is then softened, dewatered and, if it will be finished open-width, slit along a marked line so the edges stay straight.

Step 6: Drying and heat setting

A stenter dries the fabric and sets its finished width. It is a long heated frame that holds the fabric edges on pins or clips: the gap between the pin chains sets the width, overfeed lets the fabric relax lengthwise, and the heat sets polyester, nylon and spandex so their shape stays stable. Cotton is dried here but not heat-set.

Width, GSM and shrinkage move together. Stretching fabric wider lowers its GSM and stores tension that returns as shrinkage in the first wash, so finished width and GSM should be agreed as a pair; see setting weight before you sample.

At Runtang

Our finishing plant runs 16 open-width stenter lines (the machines in our mill), and finished weight and width are delivered within ±5% of the agreed specification.

Textile testing laboratory with benches and colour fastness testing equipment
Our in-house lab, where bulk specimens are tested for colour fastness, shrinkage and pilling.

Step 7: Compacting and special finishes

Compacting reduces length shrinkage by pushing the fabric together lengthwise before it is cut, much like closing an accordion. It matters most for cotton and other cellulosic knits, and it also evens out GSM.

Special finishes are added only when ordered: brushing for a lofty hand, peaching for a suede-like surface, mercerising for lustre and deeper colour on cotton, and wash effects such as mineral wash. Our plant has two mercerising lines for our mercerised cotton knit range. For what each finish changes in bulk, see what brushing, peaching and mercerising change.

Steps 8–10: Inspection, testing and packing

Every roll should be inspected and tested before it ships. Under the four-point system (ASTM D5430), each visible defect scores 1 to 4 points according to its length, and the total is converted to points per 100 square yards so rolls can be judged against an agreed limit; see how inspection limits are agreed. Specimens from the bulk lot are then tested for colour fastness to washing (ISO 105-C06), rubbing (ISO 105-X12) and perspiration (ISO 105-E04), as well as dimensional change after washing, pilling and pH.

At Runtang

Every roll is inspected with the four-point system before packing. Our in-house lab runs 11 tests on all the fabrics we produce, with specimens cut from the bulk lot and graded by at least two technicians in a light booth; see the full list of tests we run. Typical results are grade 4 to 4-5 for colour change in washing, 4 to 4-5 for light fastness on the 1–8 scale, and grade 3 or better for pilling on regular cotton knits. Deep shades on 100% cotton reach grade 3 at best for wet rubbing, which is worth allowing for in a specification. When a buyer nominates SGS, Bureau Veritas or Intertek, samples from the bulk lot are sent there too, and approved samples are kept for five years so reorders can be checked against the original.

What to specify when ordering dyed knit fabric

A clear order removes most of the guesswork from dyeing and finishing. Include:

  1. Fibre content and construction, for example 95% cotton / 5% spandex single jersey.
  2. Finished GSM and width, open-width or tubular, each with a tolerance.
  3. Colour standard and the light source for approval.
  4. Shrinkage limit, with the test method and wash conditions.
  5. Colour fastness grades for washing and rubbing.
  6. Special finishes and testing: any brushing, peaching or wash effect, and whether a third-party lab is required.

For minimum quantities and timings, see our MOQs, sampling and lead times.

FAQ

Is knit fabric dyed before or after knitting?

Usually after. Most knit fabric is knitted in greige and piece-dyed, which keeps colour lead times short; yarn is dyed first only for stripes, jacquards or heather (melange) effects.

Why does knit fabric shrink after dyeing?

Because wet processing pulls the loops lengthwise and they relax back in washing. Overfeed on the stenter and compacting remove most of this, but some residual shrinkage always remains, so buyers set a limit and a test method rather than expecting zero.

How long does bulk dyeing and finishing take?

At Runtang, bulk production takes 15–25 days, depending on the fabric and order size; lab dips take 3–5 working days.

Need knit fabric dyed to your colour standard?

Send your colour reference and fabric specification, and we will confirm the route, lab dip timing and test plan. Get a Quote

Related Articles