Condition and Mark
Measuring points are marked in length and width.
2009年創業のニット生地メーカー · 中国
試験方法 · ISO 6330 / ISO 5077
寸法変化は、生地に印を付け、ISO 6330の手順で洗濯・乾燥させ、ISO 5077で変化を算出することにより測定します。米国における同等規格はAATCC 135です。

ISO 6330の手順
ISO 5077(EN 25077)
AATCC 135
ISO 3759 sets marking, ISO 6330 the wash and dry procedure, and ISO 5077 the calculation. “Shrinkage ±5%” is only testable with the wash temperature and drying method.
Many specifications also ask for spirality (“twist”) after washing: how far the side seams or wales turn. It is tested separately from shrinkage.
Our technicians follow a written work instruction for this method.
Measuring points are marked in length and width.
Washed with the agreed ISO 6330 procedure, for example 4N at 40 °C, with ballast.
Dried as agreed: line, drip, flat or tumble.
The change is calculated as a percentage for length and width.
Key settings. Write the method and procedure in your specification.
| Parameter | Setting |
|---|---|
| Washing procedure | ISO 6330, e.g. 4N (40 °C) |
| Drying | Line, drip, flat or tumble, as agreed |
| Marking / calculation | ISO 3759 / ISO 5077 |
| Cycles | One unless specified (e.g. 3 or 5) |
| Equivalent methods | AATCC 135 (US) · GB/T 8629 / 8630 (China). Compare methods → |
Ask us for results for the selected fabric, shade and test conditions. Acceptance values for your order are agreed in writing.
Programme, temperature, drying method and number of cycles.
Knits often shrink more in length than width; set limits for each.
Compacting, relaxation and heat-setting reduce shrinkage; tell us the care label before production.
The fabric is marked (ISO 3759), washed and dried with an ISO 6330 procedure, and the change is calculated with ISO 5077.
Length and width may change by no more than 5% after the agreed wash and dry procedure. Tumble drying usually gives more shrinkage than line drying.