試験方法 · ISO 12945-1

耐ピリング性 ISO 12945-1

ISO 12945-1は、コルク張りのボックス内で回転させた後のピリングを測定するものです。一般的な綿ニットは3級以上となり、4級は非常に良好な結果です。米国の仕様ではASTM D3512がしばしば用いられます。

試験片は量産ロットから採取します。
 – Runtangカタログの生地詳細
規格

ISO 12945-1:2020(ボックス法)

米国方式

ASTM D3512 / D4970

綿ニット

3級以上、4級は非常に良好

グレード判定

1–5

01

What This Test Measures

Specimens on tubes are tumbled in a cork-lined box for an agreed number of revolutions, then compared with reference photographs in a viewing cabinet and graded from 5 (no pilling) to 1 (very severe).

The revolutions decide how hard the test is. Specifications we receive range from 7,200 to 14,400 revolutions, so a grade needs its revolutions next to it.

02

How We Run It in Our Lab

Our technicians follow a written work instruction for this method.

01

Cut and Mount

Specimens in length and width are sewn into tubes and mounted.

02

Tumble

Tubes tumble in the cork-lined box for the agreed revolutions.

03

Assess

Specimens are compared with reference photographs in a viewing cabinet.

04

Grade

Each specimen is graded 1–5 by at least two technicians.

03

Test Conditions

Key settings. Write the method and procedure in your specification.

ParameterSetting
ApparatusPilling box with cork lining
RevolutionsAs agreed, e.g. 7,200, 10,800 or 14,400
EvaluationViewing cabinet with oblique light
判定5 = no pilling, 1 = very severe
Equivalent methodsASTM D3512 / D4970 (US) · GB/T 4802.3 (China). Compare methods →
04

Measured Range and Buyer Values

Results depend on fibre, construction, shade and finishing.

Fabric / shade当社の測定範囲Values in buyer specifications
Regular 100% cotton knitsGrade 3 and above; 4 is very goodGrade 4 at 14,400 rev; 4-5 at 10,800 rev

“Our measured range” comes from our own test records on bulk lots. “Values in buyer specifications” are requirements we have received; the value that applies to your order is the one written into it. — Xiwen Zhang, Co-founder & CEO

05

Writing This Test into Your Specification

State the Revolutions

Write the grade with its revolutions, for example “grade 3-4 after 7,200 revolutions”.

Name the Instrument

Pilling box, random tumble (ASTM D3512) and Martindale give different grades.

Ask About Options

Combed or compact yarns, enzyme bio-polishing and anti-pilling finishes can raise the grade. Ask before production.

06

Questions About ISO 12945-1

What pilling grade is good for a cotton knit?

For regular 100% cotton knits, grade 3 and above in ISO 12945-1 is generally acceptable and grade 4 is a very good result.

Why does the number of revolutions matter?

More revolutions mean more abrasion; the same fabric can be grade 4 after 7,200 revolutions and grade 3 after 14,400.

Is ISO 12945-1 the same as ASTM D3512?

No. ISO 12945-1 uses a cork-lined pilling box; ASTM D3512 uses a random tumble tester. Grades are not interchangeable.